Modulus of Elasticity 0.02699 GPa
3.915 ksi
Humiseal 1A33 Urethane Conformal Coating
Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL..
Modulus of Elasticity 0.02699 GPa
3.915 ksi
Humiseal 1A33LSE Urethane Conformal Coating
Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther..