Mechanical Properties Metric English Comments
Modulus of Elasticity 2.08 GPa
302 ksi
ASTM D638
Ineos Nova 6100 Super High Impact Polystyrene  (discontinued **)
Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen..
Modulus of Elasticity 2.08 GPa
302 ksi
ASTM D638
Ineos Nova 6110 Super High Impact Polystyrene  (discontinued **)
Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen..