Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco 10 AS WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco HARRP™ 20 X 40 Wollastonite HARRP™ 20X40 is suggested for concrete and concrete roof tile reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco HARRP™ Coarse Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M15 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco MG WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD G® WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® M100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYCOR® 100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M15 Wollastonite High aspect ratio grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal perf.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® MSTPO Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® STPO Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 GPa | 43900 ksi | ASTM C848 |
CoorsTek AD-96 Alumina (nom. 96% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Modulus of Elasticity | 303 GPa | 43900 ksi | ASTM-C848 |
CoorsTek Z-PLUS™ 94 Zirconia-Impr. Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |