Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.13 GPa | 309 ksi | ISO 527-2/1A/1 |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |