Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 223 GPa | 32300 ksi | Young's Modulus |
PCC-Advanced Forming Technology 68% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |