Polymer Property : Modulus of Elasticity = 340.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.344 GPa
340.0 ksi
Kleerdex Kydex® 550 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Weatherable monolithic sheetApplications: Housings for equipment, recreational vehicles and truck parts, safety equipment, building products, signageFeatures: Kydex 550 offers the properties of "Kyd..