Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 35.0 GPa | 5080 ksi | |
Lehmann & Voss LUVOCOM® 1105-7290 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Modulus of Elasticity | 35.0 GPa | 5080 ksi | |
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Modulus of Elasticity | 35.0 GPa | 5080 ksi | |
Indium Corp. Indalloy 108 Tin-Lead Solder Alloy Good pre-tinning alloyInformation Provided by Indium Corporation |