Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 360 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.48 GPa
360 ksi
ASTM D638
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)  (Unverified Data**)
Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into..
Modulus of Elasticity 2.48 GPa
360 ksi
ISO 527
GEHR Plastics PSU Polysulfone
Polysulfone shows great thermal stability. It possesses a high mechanical strength, very good dielectric properties and hydrolysis resistance and a high radiation resistance. PSU has a low notch imp..
Modulus of Elasticity 2.48 GPa
360 ksi
ASTM D638
Ineos Nova 5190 High Impact Polystyrene  (discontinued **)
Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C ..
Copyright © lookpolymers.com All Rights Reserved