Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 260 GPa | 37700 ksi | Filament in Tension |
3M Nextel™ 720 Composite Ceramic Fiber Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 .. |