Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.268 GPa | 38.9 ksi | Molded Sample 2% Secant Modulus |
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili.. |