Polymer Property : Modulus of Elasticity = 386 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 386 GPa
56000 ksi
75° to C-axis
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam..
Modulus of Elasticity 386 GPa
56000 ksi
ASTM-C848
CoorsTek PlasmaPure-UC™ 99.9% Alumina