Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 390 GPa | 56600 ksi | ASTM E494 |
M Cubed Technologies TSC-15 Titanium-alloyed Reaction Bonded Silicon Carbide Specialty reaction-bonded SiC for applications requiring high stiffness, high toughness, and also high thermal conductivity--mechanical seals, for example Flow-through complex channels can be forme.. |
|||
Modulus of Elasticity | 390 GPa | 56600 ksi | In Tension |
Cytec Thornel® T-50 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Modulus of Elasticity | 390 GPa | 56600 ksi | In Tension |
Cytec Thornel® T-50 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |