Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.70 GPa | 682 ksi | Conditioned; ISO 178 |
Addiplast Addinyl C2 V30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Modulus of Elasticity | 4.70 GPa | 682 ksi | Conditioned; ISO 178 |
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 4.70 - 5.80 GPa @Temperature 60.0 - 150 °C |
682 - 841 ksi @Temperature 140 - 302 °F |
Average value: 5.30 GPa Grade Count:2 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Modulus of Elasticity | 4.70 - 15.5 GPa @Temperature 60.0 - 150 °C |
682 - 2250 ksi @Temperature 140 - 302 °F |
Average value: 8.93 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |