Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.75 GPa | 689 ksi | Conditioned; ISO 178 |
Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled Glass fiber reinforced, high resistance to frictionInformation provided by Addiplast. |