Mechanical Properties Metric English Comments
Modulus of Elasticity 406 GPa
58900 ksi
CMW® ELKON 100W Pure Tungsten
Tungsten, also called Wolfram, occurs as an impure tungsten oxide in wolframite and sche ores. It is chemically extracted, refined to an oxide of high purity and reduced to tungsten powder in hydrog..