Polymer Property : Modulus of Elasticity = 420.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.896 GPa
420.0 ksi
ASTM D638
Ineos Nova 1531 High Heat Crystal Polystyrene  (discontinued **)
High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p..
Modulus of Elasticity 2.896 GPa
420.0 ksi
ASTM D638
Ineos Nova 1504 High Heat Crystal Polystyrene
Good balance of flow, strength and set up properties, Blue edge effect, USP Class VIApplications: Consumer electronics, Housewares, Cosmetic packagingExposure to gamma radiation in the 2.02-6.06 meg..
Modulus of Elasticity 2.896 GPa
420.0 ksi
KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet
Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest sh..