Modulus of Elasticity 0.320 GPa
46.4 ksi
ASTM D638
Huntsman Rexell® L2102 Injection Molding LLDPE  (discontinued **)
Linear low density copolymer, injection molding, FDA compliant.Features: High flow, medium flex with good environmental stress crack (ESCR), and warpage resistance.Applications: Fitments, large lids..
Modulus of Elasticity 0.320 - 4.09 GPa

@Temperature -40.0 - 150 °C
46.4 - 593 ksi

@Temperature -40.0 - 302 °F
Average value: 1.17 GPa Grade Count:8
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..