Mechanical Properties Metric English Comments
Modulus of Elasticity 317 GPa
46000 ksi
Pacific Sintered Materials SS-410-R 410 Stainless Steel Powdered Metal
Magnetic stainless steel with high strength and good wearing properties.Equivalent MPIF Specification: SS-410-95All information provided by Pacific Sintered Metals.
Modulus of Elasticity >= 317 GPa
>= 46000 ksi
Typical minimum.
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO
Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop..
Copyright © lookpolymers.com All Rights Reserved