Mechanical Properties Metric English Comments
Modulus of Elasticity 32.0 GPa
4640 ksi
Lehmann & Voss LUVOCOM® 1-7488 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Modulus of Elasticity 32.0 GPa
4640 ksi
Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..