Mechanical Properties Metric English Comments
Modulus of Elasticity 3.31 GPa
480 ksi
ASTM D638
Ineos Nova 2580 General Purpose Crystal Polystyrene  (discontinued **)
High speed molding, Improved crack resistanceApplications: Cutlery, Consumer electronicsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optic..
Modulus of Elasticity 3.31 GPa
480 ksi
ASTM D638
Ineos Nova 2510 General Purpose Crystal Polystyrene  (discontinued **)
High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy..
Modulus of Elasticity 3.31 GPa
480 ksi
ASTM D638
Ineos Nova 2511 General Purpose Crystal Polystyrene  (discontinued **)
High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy..
Modulus of Elasticity 3.31 GPa
480 ksi
50 mm/min; ASTM D638
LG Chemical 95HC SAN Resin
Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include make-up cases and other products requiring..