Polymer Property : Modulus of Elasticity = 50.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 50.0 - 80.0 GPa
7250 - 11600 ksi
MarkeTech MC-LD and MC-MD Ultra High Temperature Machinable Ceramics
For very high temperatures or where thermal conductivity or thermal shock is important, these machinable alkaline/alkaline earth zirconium phosphate ceramics (NaZr2P3O12 or BaZr4P6O24) are recommend..
Modulus of Elasticity 50.0 - 80.0 GPa

@Temperature 1000 °C
7250 - 11600 ksi

@Temperature 1830 °F
MarkeTech MC-LD and MC-MD Ultra High Temperature Machinable Ceramics
For very high temperatures or where thermal conductivity or thermal shock is important, these machinable alkaline/alkaline earth zirconium phosphate ceramics (NaZr2P3O12 or BaZr4P6O24) are recommend..
Modulus of Elasticity 50.0 - 90.0 GPa
7250 - 13100 ksi
at constant voltage
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92)
Terfenol-D is the commercial name for Tb0.3Dy0.7Fe1.92; a composition of material that exhibits giant magnetostriction.Magnetostriction is the phenomenon in which an applied magnetic field causes an..