Polymer Property : Modulus of Elasticity = 515 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.55 GPa
515 ksi
dry
Murtfeldt Murylon® A Nylon 66
This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than..