Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 59.5 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.410 GPa
59.5 ksi
(stiffness), ASTM D882
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab..
Modulus of Elasticity 0.410 GPa
59.5 ksi
(stiffness), ASTM D882
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab..
Modulus of Elasticity 0.410 GPa
59.5 ksi
(stiffness), ASTM D882
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab..
Modulus of Elasticity 0.410 GPa
59.5 ksi
(stiffness), ASTM D882
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 150 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab..
Modulus of Elasticity 0.410 GPa
59.5 ksi
(stiffness), ASTM D882
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of ..
Modulus of Elasticity 0.410 GPa
59.5 ksi
(stiffness), ASTM D882
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of ..
Modulus of Elasticity 0.410 GPa
59.5 ksi
(stiffness), ASTM D882
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of ..
Modulus of Elasticity 0.410 GPa
59.5 ksi
(stiffness), ASTM D882
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 150 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of ..
Copyright © lookpolymers.com All Rights Reserved