Mechanical Properties Metric English Comments
Modulus of Elasticity 6.60 - 13.8 GPa
957 - 2000 ksi
Average value: 11.5 GPa Grade Count:9
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Modulus of Elasticity 6.60 - 520 GPa
957 - 75400 ksi
Average value: 105 GPa Grade Count:59
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Modulus of Elasticity 6.60 - 9.40 GPa
957 - 1360 ksi
Average value: 8.03 GPa Grade Count:10
Overview of materials for Phenolic, Resole, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of ..
Modulus of Elasticity 6.60 GPa
957 ksi
Lehmann & Voss LUVOCOM® 1105-7460/BL5019 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Chemical and hydrolysis resistance parts, non flamm..
Modulus of Elasticity 6.60 GPa
957 ksi
DIN 53 504
Dow BETAMATE™ 5103-2 Epoxy
BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated ste..
Modulus of Elasticity 6.60 - 10.9 GPa
957 - 1580 ksi
Average value: 9.31 GPa Grade Count:20
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..