Polymer Property : Modulus of Elasticity = 6.80 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 6.80 GPa
986 ksi
ISO 527-2
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 20% of glass fibers for industrial parts with high dimensional stab..