Mechanical Properties Metric English Comments
Modulus of Elasticity 42.1 GPa
6100 ksi
Indium Corp. Indalloy 128 Pure Tin
Information Provided by Indium Corporation
Modulus of Elasticity 42.1 GPa
6100 ksi
Effective Modulus
Hardwire 3x2-12-12 Medium Density Composite
The 3x2 Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3x2 wire cord is made by twisting 5 individual wire together - three straight filam..