Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.160 - 0.442 GPa | 23.2 - 64.1 ksi | Average value: 0.240 GPa Grade Count:71 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |