Mechanical Properties Metric English Comments
Modulus of Elasticity 44.8 GPa
6500 ksi
Parkway Products Thixomolded® AM50A Magnesium
Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate..
Modulus of Elasticity 44.8 GPa
6500 ksi
Parkway Products Thixomolded® AZ91D Magnesium
Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate..
Modulus of Elasticity 44.8 GPa
6500 ksi
Parkway Products Thixomolded® AM60A Magnesium
Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate..