Polymer Property : Modulus of Elasticity = 68.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 68.0 GPa
9860 ksi
Schott Glass 8245 Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and molybdenum, minimum X-ray absorption, low self radiation, good insulator X-ray tubes, video-frequency tubes, photomultiplier tubes The heavy metal..