Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 68.9 GPa | 10000 ksi | |
Potters Industries Spheriglass® 1922 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Modulus of Elasticity | 68.9 GPa | 10000 ksi | |
Potters Industries Spheriglass® 2024 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Modulus of Elasticity | 68.9 GPa | 10000 ksi | |
Potters Industries Spheriglass® 2429 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Modulus of Elasticity | 68.9 GPa | 10000 ksi | |
Potters Industries Spheriglass® 2530 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Modulus of Elasticity | 68.9 GPa | 10000 ksi | |
Potters Industries Spheriglass® 3000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Modulus of Elasticity | 68.9 GPa | 10000 ksi | |
Potters Industries Spheriglass® 5000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Modulus of Elasticity | 68.9 GPa | 10000 ksi | |
Meehanite HE Heat Resisting Cast Iron Type HE is a freely machinable material in the as-cast condition. Withstands rapid heating and cooling without premature failure, offers good dimensional stability and a good range of strength prop.. |
|||
Modulus of Elasticity | 68.9 GPa | 10000 ksi | AA 5005 |
Aleris 55HX® Aluminum (5005-H14) Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ.. |