Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.36 - 71.5 GPa | 197 - 10400 ksi | Average value: 7.82 GPa Grade Count:86 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |