Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 71.98 GPa | 10440 ksi | |
Superior Die Set FORTAL® HR Aluminum Alloy Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and d.. |