Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 88.0 GPa | >= 12800 ksi | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Modulus of Elasticity | >= 88.0 GPa @Temperature 20.0 °C |
>= 12800 ksi @Temperature 68.0 °F |
Condition T6x (Quench in water at RT) |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Modulus of Elasticity | >= 88.0 GPa | >= 12800 ksi | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Modulus of Elasticity | >= 88.0 GPa @Temperature 20.0 °C |
>= 12800 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Modulus of Elasticity | 88.0 GPa | 12800 ksi | |
Schott N-SF14 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 88.0 GPa | 12800 ksi | |
Schott N-SF8 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 88.0 GPa | 12800 ksi | |
Schott N-SSK5 Glass Information Provided by SCHOTT North America, Inc. |