Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.607 GPa | 88.0 ksi | Molded Sample 2% Secant Modulus |
Dow HDPE 04452N High Density Polyethylene DOW HDPE 04452N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and stacking strength with excellent impact strength. This resin has moderate.. |
|||
Modulus of Elasticity | 0.607 GPa | 88.0 ksi | Molded Sample 2% Secant Modulus |
Dow HDPE 25455N High Density Polyethylene DOW HDPE 25455N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and gloss with excellent toughness. This resin has good processability over a.. |