Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 88.3 GPa @Temperature 649 °C |
12800 ksi @Temperature 1200 °F |
|
AK Steel ASTM A 463 / SAE J1392 040 AHK, Grade 40 Aluminized Carbon Steel, Structural Steel (SS) Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel |
|||
Modulus of Elasticity | 88.3 GPa @Temperature 649 °C |
12800 ksi @Temperature 1200 °F |
|
AK Steel SAE J1392 050 XLK, Grade 50 Aluminized Carbon Steel, High Strength Low Alloy Steel (HSLAS) Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel |
|||
Modulus of Elasticity | 88.3 GPa @Temperature 649 °C |
12800 ksi @Temperature 1200 °F |
|
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc.. |
|||
Modulus of Elasticity | 88.3 GPa @Temperature 649 °C |
12800 ksi @Temperature 1200 °F |
|
AK Steel Aluminized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. DDS is made by adding aluminum to the molten steel and.. |
|||
Modulus of Elasticity | 88.3 GPa @Temperature 649 °C |
12800 ksi @Temperature 1200 °F |
|
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita.. |
|||
Modulus of Elasticity | 88.3 GPa @Temperature 649 °C |
12800 ksi @Temperature 1200 °F |
|
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita.. |