Polymer Property : Modulus of Elasticity = 90.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.621 GPa
90.1 ksi
Molded Sample 2% Secant Modulus
Dow DOWLEX™ IP-90 High Density Polyethylene
Next Generation DOWLEX® IP-90 resin is a high flow improved processing high density polyethylene resin designed for ultra-thin wall injection molded containers and drink cups. This resin has been m..