Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.640 - 2.20 GPa @Temperature 60.0 - 150 °C |
92.8 - 319 ksi @Temperature 140 - 302 °F |
Average value: 1.21 GPa Grade Count:1 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |