Modulus of Elasticity 66.9 GPa
9700 ksi
Parallel
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
Modulus of Elasticity 66.9 GPa
9700 ksi
Corning Macor® Machinable Glass Ceramic
The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,..
Modulus of Elasticity 66.9 GPa
9700 ksi
Accuratus MACOR Machinable Glass Ceramic
Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac..
Modulus of Elasticity 66.9 GPa
9700 ksi
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and ..