Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 1000 MPa @# of Cycles 100000 |
145000 psi @# of Cycles 100000 |
|
International Mold Steel Daido DRM1 Matrix High-Speed Steel This tough matrix type high speed tool steel features high hardness and high tough Matrix type high speed tool steel vastly surpasses hot work die steels. DRM1 improves hot and warm die life by its .. |
|||
Fatigue Strength | 1000 MPa @# of Cycles 1000 |
145000 psi @# of Cycles 1000 |
Forging with stress range 0-1000 Mpa |
TIMET TIMETAL® 829 (Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si) Titanium Alloy Weldable, High Strength, High Temperature, Creep Resistant AlloyFeatures: TIMETAL 829 combines creep resistance up to 540°C with good oxidation resistance. It is weldable and like TIMETAL 685, TIME.. |
|||
Fatigue Strength | 1000 MPa @# of Cycles 11000 |
145000 psi @# of Cycles 11000 |
Zero-to-Torsion Fatigue |
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range), Heat Treated Heat Treatment 5 hours at 527°C. 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below ar.. |