Fatigue Strength <= 780 MPa

@# of Cycles 100000
<= 113000 psi

@# of Cycles 100000
ArcelorMittal Complex Phase Steel 800 Very high strength steel, Hot Rolled Steel
Available in the following: uncoated (HCT780C) and Extragal®/Galvannealed (HCT780C+Z)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) prod..