Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 116 MPa @# of Cycles 1.00e+7 |
16800 psi @# of Cycles 1.00e+7 |
Notched, Kt=4; rotating bend (sample with UTS = 589 MPa) |
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |
|||
Fatigue Strength | 116 MPa @# of Cycles 1.00e+7 |
16800 psi @# of Cycles 1.00e+7 |
Notched, Kt=3.3; rotating bend (sample with UTS = 550 MPa) |
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |