Mechanical Properties Metric English Comments
Fatigue Strength 193 MPa

@# of Cycles 1.00e+7
28000 psi

@# of Cycles 1.00e+7
Smooth, Kt=1; rotating bend
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1)
Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties..
Fatigue Strength 193 MPa

@# of Cycles 100000
28000 psi

@# of Cycles 100000
Flexural Fatigue (SN)
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..