Polymer Property : Fatigue Strength = 21800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 150 MPa

@# of Cycles >=100000 ,
Temperature 1200 °C
21800 psi

@# of Cycles >=100000 ,
Temperature 2190 °F
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air..