Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 170 MPa @# of Cycles 1.00e+7 |
24700 psi @# of Cycles 1.00e+7 |
Notched, Kt=2; rotating bend (sample with UTS = 550 MPa) |
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |
|||
Fatigue Strength | 170 MPa @# of Cycles >=100000 , Temperature 1200 °C |
24700 psi @# of Cycles >=100000 , Temperature 2190 °F |
|
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |