Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | <= 273 MPa @# of Cycles 1.00e+8 |
<= 39600 psi @# of Cycles 1.00e+8 |
|
ArcelorMittal 04 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC04) and electroglavanized (DC04+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |