Mechanical Properties Metric English Comments
Fatigue Strength 289 MPa

@# of Cycles 1.00e+7
41900 psi

@# of Cycles 1.00e+7
notched
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + Annealed
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. ..