Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 210 MPa @# of Cycles 100000 |
30500 psi @# of Cycles 100000 |
R=0.1, Kt=2.5 |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |
|||
Fatigue Strength | 210 MPa @# of Cycles 100000 |
30500 psi @# of Cycles 100000 |
R=-1, Kt=1.75 |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |
|||
Fatigue Strength | <= 210 MPa @# of Cycles 1.00e+8 |
<= 30500 psi @# of Cycles 1.00e+8 |
|
ArcelorMittal 06 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC06) and electroglavanized (DC06+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |