Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 22.0 MPa @# of Cycles 1.00e+7 |
3190 psi @# of Cycles 1.00e+7 |
|
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |