Mechanical Properties Metric English Comments
Fatigue Strength 39.0 MPa

@# of Cycles 1000 ,
Temperature 140 °C
5660 psi

@# of Cycles 1000 ,
Temperature 284 °F
R = 0.1, 8 Hz, dry
DSM Stanyl® TW341-J PA46
Heat Stabilized, Lubricated
Fatigue Strength 39.0 MPa

@# of Cycles 1000 ,
Temperature 140 °C
5660 psi

@# of Cycles 1000 ,
Temperature 284 °F
R = 0.1, 8 Hz, dry
DSM Stanyl® TW341-N PA46
Heat Stabilized, Lubricated