Polymer Property : Fatigue Strength = 72500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 500 MPa

@# of Cycles 1.00e+6
72500 psi

@# of Cycles 1.00e+6
Zero-to-Torsion Fatigue
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range), Heat Treated
Heat Treatment 5 hours at 527°C. 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below ar..